Additive manufacturing of pure copper using ultrashort laser pulses
Authors:
- 4 March 2019
- conference paper
- Published by SPIE-Intl Soc Optical Eng
- Vol. 10909, 109090D
Abstract
Here we present laser aided additive manufacturing of pure copper parts using ultrashort laser pulses. The process is based on the powder bed fusion of pure copper powder with grain sizes in the range of 5 μm – 15 μm. For processing, a fiber laser system delivering 500 fs pulses at a wavelengths of 515 nm was used. Robust 3D printed parts are generated featuring a high degree of resolution. The fabricated copper samples were characterized in terms of morphology, density distribution, thermal and electrical conductivity. The inner structure is revealed by x-ray computed tomography measurements.Keywords
This publication has 9 references indexed in Scilit:
- Selective Laser Melting of Pure CopperJOM, 2017
- Selective laser melting of hypereutectic Al-Si40-powder using ultra-short laser pulsesApplied Physics A, 2017
- Selective laser melting of copper using ultrashort laser pulsesApplied Physics A, 2017
- Femtosecond laser additive manufacturing of iron and tungsten partsApplied Physics A, 2015
- Femtosecond laser melting and resolidifying of high-temperature powder materialsApplied Physics A, 2014
- Rapid manufacturing of metal components by laser formingInternational Journal of Machine Tools and Manufacture, 2006
- The production of copper parts using DMLRRapid Prototyping Journal, 2003
- Temperature and Finite Pulse-Time Effects in the Flash Method for Measuring Thermal DiffusivityJournal of Applied Physics, 1963
- Flash Method of Determining Thermal Diffusivity, Heat Capacity, and Thermal ConductivityJournal of Applied Physics, 1961