Influence of Cold Working and Grain Size on Pitting Corrosion Resistance of Ferritic Stainless Steel
Authors:
- 1 March 2011
- journal article
- Published by Trans Tech Publications, Ltd. in Advanced Materials Research
- Vol. 217-218, 1180-1184
Abstract
The influence of cold working and grain size on the pitting corrosion resistance of Fe-Cr-Nb-Mo ferritic stainless steel is investigated using optical microscope and electrochemical methods. The pitting corrosion resistance firstly decreases with increasing the cold-rolling reduction from 0% to 30% due to the number of nucleation site increasing. With increasing the cold-rolling reduction from 40% to 60%, the disappearance of grain boundaries, stacked dislocation and uniform microstructure results in the pitting corrosion resistance of the steel. With prolonging the annealing time, the grain size of the steel grows, and the pitting potential of the steel decrease. The smaller grain size promotes the formation of compact passive film and improves the pitting corrosion resistance.Keywords
This publication has 7 references indexed in Scilit:
- Microstructure and mechanical properties of 12wt.% Cr ferritic stainless steel with Ti and Nb dual stabilizationMaterials & Design (1980-2015), 2009
- Effects of light pre-deformation on pitting corrosion resistance of copper-bearing ferrite antibacterial stainless steelJournal of Materials Processing Technology, 2008
- An alternate explanation for the abrupt current increase at the pitting potentialCorrosion Science, 2008
- Influence of Cold Work on Pitting Corrosion Behavior of a High Nitrogen Stainless SteelJournal of the Electrochemical Society, 2008
- Influence of cold working on the pitting corrosion resistance of stainless steelsCorrosion Science, 2007
- Grain size dependence of mechanical, corrosion and tribological properties of high nitrogen stainless steelsJournal of Materials Science, 2003
- Effect of alloying Cu on the corrosion resistance of stainless steels in chloride mediaCorrosion Science, 2001