Model for thickness dependence of mobility and concentration in highly conductive zinc oxide
Authors:
Open Access
- 1 March 2013
- journal article
- Published by SPIE-Intl Soc Optical Eng in Optical Engineering
- Vol. 52 (3) , 033801
Abstract
The dependences of the 294 and 10 K mobility and volume carrier concentration on thickness ( to 147 nm) are examined in aluminum-doped zinc oxide (AZO). Two AZO layers are grown at each thickness, one with and one without a 20-nm-thick ZnON buffer layer. Plots of the 10 K sheet concentration versus for buffered (B) and unbuffered (UB) samples give straight lines of similar slope, and , but different -axis intercepts, and , respectively. Plots of versus at 294 K produce substantially the same results. Plots of versus can be well fitted with the equation , where is the thickness for which is reduced by a factor 2. For the B and UB samples, and 23 nm, respectively, showing the efficacy of the ZnON buffer. Finally, from and we can use degenerate electron scattering theory to calculate bulk donor and acceptor concentrations of and , respectively, and Drude theory to predict a plasmonic resonance at 1.34 μm. The latter is confirmed by reflectance measurements.
Keywords
Funding Information
- AFOSR (FA9550-10-1-0079)
- NSF (DMR0803276)
- DOE (DE-FG02-11ER46820)