Syntactic foam composites containing 0, 0.9, 1.76, 2.54, 3.54, and 4.5 vol % of E‐glass fibers in the form of chopped strands were fabricated and subjected to compression testing. It was found that the compressive strength values generally increased with fiber content except for the 3.54% fiber‐bearing cast slab, which recorded lower values. This lone exception was due to the difference in processing route adopted in fabricating this particular fiber‐bearing foam. Also noticed was the fact that the compressive strength of the 0.9 vol % fiber‐bearing system was lower compared to the fiber‐free system. This was correlated to the higher level of void content noticed with this fiber‐bearing foam compared to that seen in the unreinforced foam. © 2001 John Wiley & Sons, Inc. J Appl Polym Sci 81: 405–411, 2001Keywords
This publication has 8 references indexed in Scilit:
- Characterization of reinforced syntactic foams using ultrasonic imaging techniqueBulletin of Materials Science, 1999
- Composite sandwich construction with syntactic foam coreComposites, 1993
- Use of Syntactic Foams for Subsea BuoyancyCellular Polymers, 1991
- Syntactic polymer foams1986
- Syntactic Foams I. Preparation, Structure and PropertiesJournal of Cellular Plastics, 1980
- Phase Relationship in Three-Phase Composites Which Include a Void PhaseJournal of Composite Materials, 1976
- Mechanical Properties and Characterization of Phenolic Resin Syntactic FoamsJournal of Cellular Plastics, 1974
- Preparation of syntactic carbon foamCarbon, 1972