Influence of Carbon Cloth Filaments Upon the Properties of 2D C/SiC via Precursor Infiltration and Pyrolysis Process

Authors:

Abstract
In this paper, 2D C/SiC composites with different carbon cloth filaments (1K, 3K) were prepared via precursor infiltration and pyrolysis (PIP) process. The flexural strength of 2D-1K C/SiC composites was 380MPa, and fracture toughness was 16.8MPa-m1/2, while those of 2D-3K C/SiC were 305MPa and 14.4MPa-m1/2, respectively. The differences of these two composites were analyzed from fiber volume ratio in the composites, density, and fracture surface (SEM) of the samples.