Controlling of reheated quenching temperature of 1000 MPa grade steel plate for hydropower station
Authors:
- 15 January 2019
- journal article
- research article
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 50 (1) , 33-43
Abstract
The strength and toughness of 1000 MPa grade steel plate for hydropower station treated by different reheated quenching temperatures were investigated. With the increasing of reheated quenching temperature, the yield strength and tensile strength increase sharply, whereas the value of impact toughness decreases slowly. The lath martensite with high density dislocations enhances dislocation strengthening. On the contrary, the acicular or block ferrite (soft phase) produced by intercritical quenching reduces the phase transformation strengthening. Moreover, the ferrite has a low solubility of interstitial carbon due to the body‐centered‐cubic lattice structure. The bar‐shaped precipitates occur during the isothermal holding at the intercritical temperature and it will reduce the precipitation strengthening. The ferrite phase and high misorientation boundaries are the main factors that contribute to the toughening of the experimental steel. The lower the reheated quenching temperature is, the higher proportion of ferrite and high misorientation boundaries becomes. Considering the requirements for mechanical properties of 1000 MPa grade steel plate for hydropower station, the optimal temperature of reheated quenching is ∼920 °C.Keywords
Funding Information
- National Natural Science Foundation of China and Baowu Steel Group Co. Ltd (U1660205)
This publication has 26 references indexed in Scilit:
- Effect of Quenching Process on Microstructures and Mechanical Properties of Fe-0.9Mn-0.5Cr-2.4Ni-0.5Mo-C SteelJournal of Materials Engineering and Performance, 2018
- Effect of quenching temperature on martensite multi-level microstructures and properties of strength and toughness in 20CrNi2Mo steelMaterials Science and Engineering: A, 2016
- Effect of Martensite Morphology on Impact Toughness of Ultra-High Strength 25CrMo48V Steel Seamless Tube Quenched at Different TemperaturesJournal of Iron and Steel Research International, 2013
- Micro-tension behaviour of lath martensite structures of carbon steelMaterials Science and Engineering: A, 2013
- Microstructural characteristics and impact fracture behavior of a high-strength low-alloy steel treated by intercritical heat treatmentMaterials Science and Engineering: A, 2012
- Analysis of martensite–austenite constituent and its effect on toughness in submerged arc welded joint of low carbon bainitic steelJournal of Materials Science, 2012
- Effect of Substructure on Toughness of Lath Martensite/Bainite Mixed Structure in Low-Carbon SteelsJournal of Iron and Steel Research International, 2010
- Effect of welding heat input on microstructure and mechanical properties of simulated HAZ in Cu containing microalloyed steelJournal of Materials Science, 2009
- The morphology and crystallography of lath martensite in Fe-C alloysActa Materialia, 2003
- The Application and the Problems of High Strength Steel on Penstock in Chinese Hydroelectric Station.ISIJ International, 2002