Enhancing torsion fatigue behaviour of a martensitic stainless steel by generating gradient nanograined layer via surface mechanical grinding treatment
Authors:
- 1 October 2013
- journal article
- Published by SAGE Publications in Materials Science and Technology
- Vol. 29 (10) , 1200-1205
Abstract
A gradient nanograined (GNG) surface layer was formed on a martensitic stainless steel bar sample by means of the surface mechanical grinding treatment (SMGT). The average grain size is ∼25 nm on the topmost surface layer and increases gradually with increasing depth. The torsion fatigue strength is elevated by 38 with the GNG surface layer compared with the original material. An additional 8 increment in fatigue strength is achieved after a post-annealing treatment of the SMGT sample. By analysing the microstructure, hardness, surface roughness and residual stress distribution in the SMGT samples, we believe that the enhanced fatigue resistances originate from the GNG structure with a hard surface layer and a high structural homogeneity.Keywords
This publication has 30 references indexed in Scilit:
- Grain size effects on the austenitization process in a nanostructured ferritic steelActa Materialia, 2011
- Superficial severe plastic deformation of 316 LVM stainless steel through grit blasting: Effects on its microstructure and subsurface mechanical propertiesSurface and Coatings Technology, 2010
- The effects of deep rolling and shot peening on fretting fatigue resistance of Aluminum-7075-T6Materials Science and Engineering: A, 2009
- Fatigue life behaviour of the dual-phase low carbon steel sheetsJournal of Materials Processing Technology, 2009
- Effect of structure evolution induced by ultrasonic peening on the corrosion behavior of AISI-321 stainless steelMaterials Science and Engineering: A, 2007
- Fatigue behavior of nanocrystalline metals and alloysInternational Journal of Fatigue, 2005
- An approach for prediction of fatigue strength of shot peened componentsEngineering Fracture Mechanics, 2004
- On the influence of mechanical surface treatments—deep rolling and laser shock peening—on the fatigue behavior of Ti–6Al–4V at ambient and elevated temperaturesMaterials Science and Engineering: A, 2003
- Crack closure and crack growth behaviour in shot peened fatigued specimenEngineering Fracture Mechanics, 1999
- Theory of Elasticity (3rd ed.)Journal of Applied Mechanics, 1970