High Throughput SiC Wafer Polishing with Good Surface Morphology
Authors:
- 15 September 2007
- journal article
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 556-557, 753-756
Abstract
We report SiC wafer polishing study to achieve high throughput with extremely flat, smooth and damageless surface. The polishing consists of three process, wafer grinding, lapping and chemical mechanical polishing (CMP), which are completed in shortest about 200 minutes in total for 2 inch wafer. Specimens of 4H- and 6H-SiC were provided from slicing single crystal as wafers oriented (0001) with 0 or 8 degrees offset angle toward to . By the first grinding using a diamond whetstone wheel, we realized flat surface on the wafers with small TTV error of 1 μm in 15 minutes. After second process of lapping, the wafers were finished by CMP using colloidal silica slurry. AFM observation showed not only scratch-free surface but also atomic steps on the wafers after CMP. Rms marks extremely flat value of 0.08 nm in 10 μm square area.Keywords
This publication has 5 references indexed in Scilit:
- Large Diameter and Long Length Growth of SiC Single CrystalMaterials Science Forum, 2004
- Chemomechanical Polishing of Silicon CarbideJournal of the Electrochemical Society, 1997
- Characterization of Polishing‐Related Surface Damage in (0001) Silicon Carbide SubstratesJournal of the Electrochemical Society, 1995
- Mechanochemical Polishing of Silicon Carbide Single Crystal with Chromium(III) Oxide AbrasiveJournal of the American Ceramic Society, 1992
- Super-polished silicon carbide mirror for high-power operation of excimer lasers in a vacuum ultraviolet spectral rangeReview of Scientific Instruments, 1990