POROSITY, PERMEABILITY AND MICROSTRUCTURE OF FOAMED CONCRETE THROUGH SEM IMAGES
Authors:
- P. ShawnimPSP. Shawnim
- F. MohammadFMF. Mohammad
Open Access
- 25 April 2019
- journal article
- Published by UNIMAS Publisher in Journal of Civil Engineering, Science and Technology
- Vol. 10 (1) , 22-33
Abstract
This paper examined the foamed concrete (FC) for permeability of total and capillary water absorption, at 28 days of air sealed curing. The microstructure of 15 selected FC specimens was investigated to determine permeability in relation to porosity and density using Scanning Electron Microscopy (SEM) images. The FC specimens of the densities (1100, 1600, and 1800) kg/m3 were made using fine sand and brick aggregates with toner and MK inclusion as additives. The microstructural investigation of the FC revealed, porosity measure as a percentage ratio of the area under investigation to be in the range of (39.65 to 77.7) %. The pore size is in the range of (0.01 to 70) µm, depending on the type of additive, for the mixes containing toner and MK, it is in a fine range of (0.01 to 10.0) µm. For the FC specimens, the finer the pore size, the less permeable and the stronger it is. Permeability is porosity and strength dependent, whereby high porosity leads to high permeability and low compressive strength for FC mixes made with sand or brick only with no additive inclusion. Meanwhile, the FC mixes made with the inclusion of additives, such as the toner and MK20 mixes, showed an evenly spread net of independent air voids with a regular shape within their matrix, which is beneficial in decreasing permeability. Therefore, besides the porosity and strength, the fineness of the pore matrix and the shape factor of the pores are two other key factors in controlling permeability. Toner and MK20 inclusion can enhance the capillary water absorption to reach almost water tight. Besides, MK30 and MK50 inclusion displayed adverse effect on permeability. Depending on the type of filler, the additive, and the percentage ratio of the porosity of the FC matrix at (1600 and 1800) kg/m3 densities, it is possible to produce FC with compressive strength between (55.1 and 30) N/mm2.Keywords
This publication has 25 references indexed in Scilit:
- Pore Structure and Microstructure of Foam ConcreteAdvanced Materials Research, 2010
- Mechanical properties of brick aggregate concreteConstruction and Building Materials, 2009
- The use of coarse and fine crushed bricks as aggregate in concreteConstruction and Building Materials, 2008
- Sorption characteristics of foam concreteCement and Concrete Research, 2007
- Air‐void characterisation of foam concreteCement and Concrete Research, 2007
- Heat of hydration in foamed concrete: Effect of mix constituents and plastic densityCement and Concrete Research, 2006
- Influence of fly ash fineness on strength, drying shrinkage and sulfate resistance of blended cement mortarCement and Concrete Research, 2004
- Environmentally-friendly mortars: a way to improve bond between mortar and brickMaterials and Structures, 2003
- Pore size distribution of metakaolin pasteCement and Concrete Research, 1996
- Image analysis techniques for characterization of pore structure of cement-based materialsCement and Concrete Research, 1994