Abstract
The low temperature stress corrosion cracking of sensitized Inconel 600 has been examined using aerated 1.3% boric acid solutions with small additions of sodium thiosulfate. Cracking is observed for thiosulfate concentrations above 10−6 M. The rate of cracking increases with temperature to at least 80 C. Concentrated solutions with potential control give crack velocities up to about 0.4 μm/s at 22 C. Provided that cracks are initiated by slow straining, they continue to propagate at very low apparent stress intensities. Lithium hydroxide additions inhibit SCC by producing borate anions; the rate of borate to thiosulfate ion concentration is an important factor in determining immunity to SCC.Keywords
This publication has 7 references indexed in Scilit:
- Stress-corrosion cracking of sensitized type 304 stainless steel in thiosulfate solutionsMetallurgical Transactions A, 1982
- The Stress Corrosion Cracking of Sensitized Stainless Steel in Thiosulfate SolutionsCorrosion, 1982
- Resistance to Flow of Current to Scratched ElectrodesJournal of the Electrochemical Society, 1981
- Materials Requirements for Pressurized Water Reactor Steam Generator TubingNuclear Technology, 1981
- Transport Processes and the Mechanism of Pitting of MetalsJournal of the Electrochemical Society, 1976
- The initiation of intergranular failure in inconel-600Metallurgical Transactions, 1971
- The Corrosion of Materials in Reactor Containment Spray SolutionsNuclear Technology, 1971