A PROCEDURE FOR ANALYSIS OF LEAK BEFORE BREAK IN PIPES SUBJECTED TO FATIGUE OR IGSCC ACCOUNTING FOR COMPLEX CRACK SHAPES
Authors:
- 1 October 1995
- journal article
- Published by Wiley in Fatigue & Fracture of Engineering Materials & Structures
- Vol. 18 (10) , 1173-1188
Abstract
A procedure is described which predicts the growth of an initial circumferential surface crack through a pipe wall and further on to final failure of the pipe. The crack growth mechanism can either be fatigue or stress corrosion. Consideration is taken to complex crack shapes, since especially the last growth mechanism often results in a substantially longer crack length on the inside of the pipe than on the outside for the initial leaking crack due to the distribution of weld residual stresses. The procedure has been implemented in a computer program that in an integrated fashion calculates crack sizes and mass leak rates as a function of time and also predicts when leakage and final failure occur. The information obtained makes it possible to judge if the concept of leak before break is fulfilled.Keywords
This publication has 13 references indexed in Scilit:
- FATIGUE LIFE AND PENETRATION BEHAVIOUR OF A SURFACE‐CRACKED PLATE UNDER COMBINED TENSION AND BENDINGFatigue & Fracture of Engineering Materials & Structures, 1994
- Finite element analysis of limit loads for surface cracks in platesInternational Journal of Pressure Vessels and Piping, 1994
- Near-tip field characterization and J-integral evaluation for nonproportional loadsInternational Journal of Solids and Structures, 1994
- LEAK‐BEFORE‐BREAK CONDITIONS OF PLATES AND PIPES UNDER HIGH FATIGUE STRESSESFatigue & Fracture of Engineering Materials & Structures, 1992
- A consistent few parameter crack growth description procedureInternational Journal of Fracture, 1992
- Stress intensity factors and influence functions for circumferential surface cracks in pipesEngineering Fracture Mechanics, 1991
- Elastic crack opening displacements and rotations in through-cracks in spheres and cylinders under membrane and bending loadingEngineering Fracture Mechanics, 1986
- Technical report on material selection and processing guidelines for BWR coolant pressure boundary piping. Draft report. Revision 21986
- Fracture behavior of cracked Type 304 stainless steel pipes under tensile and thermal loadingsInternational Journal of Pressure Vessels and Piping, 1985
- Stress Intensity Factors, Crack Profiles, and Fatigue Crack Growth Rates in Residual Stress Fields1982