Contact Damage Resistance and Strength Degradation of Glass-infiltrated Alumina and Spinel Ceramics
Authors:
- 1 March 1999
- journal article
- research article
- Published by SAGE Publications in Journal of Dental Research
- Vol. 78 (3) , 804-814
Abstract
All-ceramic crowns are coming into widespread use because of their superior esthetics and chemical inertness. This study examines the hypothesis that glass-infiltrated alumina and spinel core ceramics are resistant to damage accumulation and strength degradation under representative oral contact conditions. Accordingly, Hertzian indentation testing with hard spheres is used to evaluate damage accumulation in alumina and spinel ceramics with different pre-form grain morphologies and porosities. Indentation stress-strain curves measured on fully infiltrated materials reveal a marked insensitivity to the starting pre-form state. The glass phase is shown to play a vital role in providing mechanical rigidity and strength to the ceramic structures. All the infiltrated ceramics show subsurface cone fracture and quasi-plastic deformation above critical loads Pc (cracking) and Py (yield), depending on sphere radius, with Py < Pc. Strength degradation from accumulation of damage in Hertzian contacts above these critical loads is conspicuously small, suggesting that the infiltrated materials should be highly damage-tolerant to the "blunt" contacts encountered during mastication. Failure in the strength tests originates from either cone cracks ("brittle mode") or yield zones ("quasi-plastic mode"), with the brittle mode more dominant in the spinels and the quasi-plastic mode more dominant in the aluminas. Multi-cycle contacts at lower loads, but still above loads typical of oral function, are found to be innocuous up to 105 cycles in air and water, although contacts at 106 cycles in water do cause significant strength degradation. By contrast, contacts with Vickers indenters produce substantial strength losses at low loads, suggesting that the mechanical integrity of these materials may be compromised by inadvertent "sharp" contacts.Keywords
This publication has 24 references indexed in Scilit:
- CERAMICS IN RESTORATIVE AND PROSTHETIC DENTISTRYAnnual Review of Materials Science, 1997
- Indentation fatiguePhilosophical Magazine A, 1993
- Postfailure subsidiary cracking from indentation flaws in brittle materialsJournal of Materials Research, 1993
- Sharp vs Blunt Crack Hypotheses in the Strength of Glass: A Critical Study Using Indentation FlawsJournal of the American Ceramic Society, 1985
- A Critical Evaluation of Indentation Techniques for Measuring Fracture Toughness: I, Direct Crack MeasurementsJournal of the American Ceramic Society, 1981
- Strength Degradation of Brittle Surfaces: Sharp IndentersJournal of the American Ceramic Society, 1976
- Strength Degradation of Brittle Surfaces: Blunt IndentersJournal of the American Ceramic Society, 1975
- A Study of Dislocation Arrays at Spherical Indentations in LiF as a Function of Indentation Stress and StrainPhysica Status Solidi (b), 1969
- Pulse Superposition Method for Measuring Ultrasonic Wave Velocities in SolidsThe Journal of the Acoustical Society of America, 1961
- The deformation of metals by vickers-type pyramidal indentersJournal of the Mechanics and Physics of Solids, 1959