Anodic Polishing of Plain Carbon Steels

Authors:
  • RIRobert L. Imboden
    Robert L. Imboden
  • RSRobert S. Sibley
    Robert S. Sibley

Abstract
Specimens of low carbon steels, previously prepared on 3/0 metallographic paper for metallographic study, were anodically polished and etched. Five electrolytic baths were found satisfactory, three of which gave excellent results. One bath, composed of 40% sulfuric acid, 46% phosphoric acid, 4% dextrose, 10% water, used a current density of 1.5 to 4.5 amp./sq. in. (23 to 70 amp./dm.2), bath temp. of 28 to 40° C., and 5 to 10 minutes for polishing. Another bath, composed of 15% sulfuric acid, 65% phosphoric acid, 5% chromic acid, and 15% water, used 3 to 7 amp./sq. in. (47 to 109 amp./dm.2), bath temp. of 42 to 55° C., and 3 to 5 minutes for polishing. The third bath was organic, 765 cc. acetic anhydride, 185 cc. perchloric acid, 50 cc. water, 0.25 to 0.8 amp./sq. in. (3.9 to 12.5 amp./dm.2), bath temp. below 30° C., and 5 to 10 minutes for optimum polishing. Etching of the samples occurred at slightly lower current densities. Theory of electropolishing is discussed covering (1) preferential removal of scratch ridges; (2) longer time required by vigorous agitation; (3) formation of undulations; (4) pitting around surface inclusions; and (5) mechanical polishing vs. electropolishing. Types of cells applicable for preparation of samples for metallographic study are shown. It is important to perform a two‐dimensional study on the specimens if a true metallographic history of the sample is desired. Sixteen micrographs are shown.