NaCl Induced High Temperature Corrosion of Alloy 625 Fabricated by Laser Metal Deposition – Powder
Authors:
Preprint
- 7 August 2024
- preprint
- Published by Springer Nature in Research Square
Abstract
The present study describes the corrosion behavior of alloy 625 fabricated by Laser Metal Deposition-powder in the presence of a solid NaCl deposit in laboratory air at 650 and 800°C. The results showed that at both temperatures, the presence of the deposit had a catastrophic effect on the corrosion resistance of the alloy. The active corrosion mechanism resulted in a very thick and non-protective oxide scale and in a highly damaged metal zone beneath the oxide scale. Although the mechanism involved was the active corrosion mechanism at both 650 and 800°C, differences were observed between these two temperatures. At 800°C, the corrosion products were thicker, and the substrate was significantly more damaged, especially due to the formation of an interconnected network of voids. At 650°C, the thick and continuous Cr2O3 layer, predominantly observed at 800°C, was not present. The use of thermodynamic data helped to suggest possible explanations for the observed differences. Overall, the increase of temperature accelerated the degradation of the alloy and it was enhanced by a radical change of the main reactions of the active corrosion mechanism between 650 and 800°C.Keywords
All Related Versions
This publication has 22 references indexed in Scilit:
- High Temperature Oxidation of Additively Manufactured Structural AlloysJOM, 2022
- High-temperature oxidation performance of Inconel 625 superalloy fabricated by wire arc additive manufacturingCorrosion Science, 2022
- A comparison of the high-temperature oxidation behaviour of conventional wrought and laser beam melted Inconel 625Corrosion Science, 2020
- Waste incineration corrosion processes: Oxidation mechanisms by electrochemical impedance spectroscopyMaterials and Corrosion, 2008
- The role of alloying elements in commercial alloys for corrosion resistance in oxidizing‐chloridizing atmospheres. Part II: Experimental investigationsMaterials and Corrosion, 2003
- The effects of chlorides, hydrogen chloride, and sulfur dioxide in the oxidation of steels below depositsCorrosion Science, 1995
- The performance of Alloy 625 in long-term intermediate temperature applicationsInternational Journal of Pressure Vessels and Piping, 1994
- Effects of alloying elements on NaCl-induced hot corrosion of stainless steelsMaterials Science and Engineering: A, 1989
- Ignition of nickel in environments containing oxygen and chlorineMetallurgical Transactions A, 1987
- Halogen Corrosion of Metals1976