Abstract
This study investigates the formation sequence and growth kineticsof intermetallic compounds (IMCs) during the reaction between liquidaluminum (Al) and solid iron (Fe), using for the first time both in situsynchrotron X-ray diffraction and tomography with samples designed totailor the morphology of the reaction interface.Experimental samples comprised commercially pure mixtures of Al and Fe powders, as well asAl powders deposited onto Fe rods, annealed at temperatures ranging from400 °C to 900 °C. Two primary IMC phases—Fe2 Al5 and Fe4 Al13 —weresystematically observed during annealing, appearing simultaneously as soonas Al melted, with Fe2 Al5 as the dominant phase, exhibiting its characteristictongue-like morphology. A temperature ramp applied to the powder mixturefurther revealed the subsequent formation of FeAl, followed by FeAl2 . Themultisite and multidirectional reaction front of the powder mixture samplelead to very fast growth of the IMCs, consuming most of the reactants withina few tens of seconds. Conversely for the Al/Fe rod configuration (featuringa single reaction interface), the steady increase in IMC layer thickness wasmonitored in situ and confirmed to follow a volume-diffusion-controlledgrowth regime at 700 °C, with derived diffusion parameters: pre-exponentialfactor k0 = 8.43 · 10-2 m2 s-1 and activation energy Q = 187 kJ mol-1 .However, at 770 °C and 830 °C, the kinetics deviated from this regime afteran initial time delay, due to liquid Al dissolving the IMC layer. Beyondreducing layer thickness, this dissolution also induced Fe4 Al13 precipitationwithin the Al matrix upon cooling. Tracking the displacement of the Fe/IMCand Al/IMC interfaces additionally demonstrated that Fe repels the IMCtoward liquid Al, a mechanism proposed to minimize transformation-inducedstress, scaling with the molar volume mismatch between Fe and Fe2 Al5 .

This publication has 39 references indexed in Scilit: