Effect of hydrogen on the unintentional doping of 4H silicon carbide
- 21 October 2022
- journal article
- conference paper
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 132 (15) , 155704
Abstract
High-purity semi-insulating (HPSI) 4H silicon carbide (4H-SiC) single crystals are critical semiconductor materials for fabricating GaN-based high-frequency devices. One of the major challenges for the growth of HPSI 4H-SiC single crystals is the unintentional doping of nitrogen (N) and boron (B). The addition of hydrogen has been supposed to mitigate unintentional doping. However, the underlying mechanism has not been well understood. In this work, the role of hydrogen in the growth of HPSI 4H-SiC single crystals is investigated by first-principles formation-energy calculations. We find that the addition of hydrogen significantly mitigates N doping while hardly affecting B doping. Once hydrogen is added, hydrogen may adsorb at the growing surface of 4H-SiC, leading to surface passivation. Since N can react with hydrogen to form stable NH3 (g), the chemical potential of N is reduced, so that the formation energy of N in 4H-SiC increases. Hence, the critical partial pressure of nitrogen required for the growth of HPSI 4H-SiC single crystals increases by two orders of magnitude. Moreover, we reveal that the adjustment of relative B and N doping concentrations has a substantial impact on the Fermi energy of HPSI 4H-SiC. When the doping concentration of N is higher than that of B, N interacts with carbon vacancies (VC) to pin the Fermi energy at Z1/2. When the doping concentration of B is higher than that of N, the Fermi energy is pinned at EH6/7. This explains that the resistivity of unintentionally doped HPSI 4H-SiC may vary.Keywords
Funding Information
- Foundation for Innovative Research Groups of the National Natural Science Foundation of China (91964107)
- Foundation for Innovative Research Groups of the National Natural Science Foundation of China (U20A20209)
- Foundation for Innovative Research Groups of the National Natural Science Foundation of China (61721005)
This publication has 34 references indexed in Scilit:
- Deep Levels Observed in High-Purity Semi-Insulating 4H-SiCMaterials Science Forum, 2010
- Wide gap semiconductor microwave devicesJournal of Physics D: Applied Physics, 2007
- Growth of 6H-SiC crystals with low boron concentrationJournal of Crystal Growth, 2006
- Properties of 6H–SiC crystals grown by hydrogen-assisted physical vapor transportApplied Physics Letters, 2005
- Overcoming the doping bottleneck in semiconductorsComputational Materials Science, 2004
- Defects in High-Purity Semi-Insulating SiCMaterials Science Forum, 2004
- On the preparation of vanadium doped PVT grown SiC boules with high semi-insulating yieldJournal of Crystal Growth, 2003
- Understanding Ultrahigh Doping: The Case of Boron in SiliconPhysical Review Letters, 2003
- SiC materials-progress, status, and potential roadblocksProceedings of the IEEE, 2002
- An Investigation of the Compound Silicon Boride (SiB[sub 6])Journal of the Electrochemical Society, 1959