Structural Ceramic Microlaminates by Electrophoretic Deposition

Authors:

Abstract
Yttria‐stabilized zirconia (YSZ)/Al 2 O 3 laminar microcomposites with a total of 80 layers, each as thin as ∼2 μm, were fabricated by electrophoretic deposition. Positively charged YSZ or Al 2 O 3 powders were deposited on a cathode, layer by layer from 10 wt% solids/ethanol suspensions. The suspensions were characterized by their rate of deposition as a function of voltage. The deposited samples had a green density of ∼60% of theoretical. The microstructure of the sintered, theoretically dense samples was characterized by optical and electron microscopy, and microindentation was used to explore the mechanical properties.

This publication has 13 references indexed in Scilit: