Growth behavior and mechanism of tin whisker on isolated SnAg solder under compressive stress
- 8 April 2021
- conference paper
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 1-3
Abstract
Tin whisker growth on microbumps is a risk to the reliability of electrical devices. In this paper, three types of reflowed microbumps were under 16 MPa compressive stress at 25, 55 and 85°C for 5 days. The growth behavior of tin whisker analyzed and interpreted by the Power law creep mechanism. The tin whisker growth of microbump solder mainly at the twin boundary nucleation site followed dislocation creep mechanism at 25°C.Keywords
Funding Information
- National Natural Science Foundation of China (51991374)
- National Basic Research Program of China (2015CB057200)
This publication has 11 references indexed in Scilit:
- Recent advances on kinetic analysis of solder joint reactions in 3D IC packaging technologyMaterials Science and Engineering: R: Reports, 2019
- Evidence of 3D strain gradients associated with tin whisker growthScripta Materialia, 2018
- Microscale deformation behavior of bicrystal boundaries in pure tin (Sn) using micropillar compressionActa Materialia, 2016
- Sn whisker evaluations in 3D microbumped structuresMicroelectronics Reliability, 2014
- Corrosion behavior of pure tin deposit under 55 °C/85 % RH reliability testJournal of Materials Science: Materials in Electronics, 2013
- Effect of Crystal Orientation on Mechanically Induced Sn Whiskers on Sn-Cu PlatingJournal of Electronic Materials, 2012
- Co-W as an advanced barrier for intermetallics and electromigration in fine-pitch flipchip interconnections2011
- Review and Analysis of Lead‐Free Solder Material Properties2007
- Spontaneous growth mechanism of tin whiskersActa Materialia, 1998
- Temperature dependence of the grain boundary diffusion of tin in nickelActa Metallurgica, 1987