Abstract
Surface passivation of crystalline silicon (c-Si) is experimentally studied during the growth of a hydrogenated amorphous silicon (a-Si:H) and epitaxial silicon (epi-Si) passivation layer at a subnanometer to nanometer scale. The property of surface passivation is monitored in real time via in situ measurement of a photocurrent in c-Si under plasma-enhanced vapor deposition for the passivation layer growth. The measurement results suggest the following. Passivation is improved by the growth of an a-Si:H layer, where a large band offset is formed at the a-Si:H/c-Si interface, and the carrier recombination is suppressed. On the other hand, passivation is deteriorated with the growth of an ultrathin epi-Si layer ( d ≲ 2.5 ± 1.0 nm) because the band offset is not formed at the interface, and plasma-induced defects are created in c-Si. However, passivation is improved with a thick epi-Si layer ( d ≳ 2.5 ± 1.0 nm), where the band bending is formed near the epi-Si/c-Si interface, which partially suppresses the carrier recombination. The suppression of the plasma-induced defects as well as the formation of the band offset are important for surface passivation.
Funding Information
  • Japan Society for the Promotion of Science (18K03603)
  • Japan Society for the Promotion of Science (20H00142)
  • New Energy and Industrial Technology Development Organization

This publication has 71 references indexed in Scilit: