Early localized corrosion of 2219-T8 aluminum alloy for liquid-propellant tanks under accelerated nitric-acid exposure: Al-selective dealloying of θ-Al₂Cu

Authors:

Abstract
Localized corrosion of 2219-T8 aluminum alloy may compromise the surface integrity of liquid-propellant tanks when trace moisture in N₂O₄ produces nitric-acid-related corrosive species. To clarify the earliest microstructural damage involved in this process, the alloy was exposed to 25 wt.% HNO₃ at 25 °C and examined by integrating electrochemical measurements, correlative microscopy, surface-topography characterization and first-principles calculations. Early localized attack concentrated at chemically heterogeneous θ-Al₂Cu/matrix regions. Preferential removal of Al from these regions produced porous Cu-enriched remnants, demonstrating early Al-selective dealloying of θ-Al₂Cu. Meanwhile, subsurface cavities and localized material loss developed near precipitate/matrix interfaces, progressively reducing precipitate support and promoting local destabilization within the first hour of exposure. Continued growth and interaction of these damaged regions subsequently transformed isolated pits into connected trench-like surface features. The experimentally observed selectivity toward Al-rich environments was rationalized by the consistently stronger nitrate-related adsorption, lower work functions and greater charge transfer calculated for Al(110) and Al-terminated θ-Al₂Cu(001) than for Cu-terminated θ-Al₂Cu(001). These results show a sequential damage pathway in which preferential interaction and dissolution at Al-rich sites drive θ-Al₂Cu dealloying and interfacial degradation, and the resulting precipitate destabilization promotes pit coalescence. The findings show that Al-rich θ-Al₂Cu-associated environments are early microstructural vulnerabilities of 2219-T8 propellant-tank alloy under accelerated nitric-acid exposure relevant to moisture-affected N₂O₄ conditions.

This publication has 27 references indexed in Scilit: