Effect of Different Ceramic Surface Treatments on Resin Microtensile Bond Strength
Authors:
- Alfredo Meyer FilhoAFAlfredo Meyer Filho
- Luiz Clovis Cardoso VieiraLVLuiz Clovis Cardoso Vieira
- Élito AraújoÉAÉlito Araújo
- Sylvio Monteiro JúniorSJSylvio Monteiro Júnior
- 1 March 2004
- journal article
- Published by Wiley in Journal of Prosthodontics
- Vol. 13 (1) , 28-35
Abstract
Purpose:The objective of this study was to evaluate the effect of different surface treatments on the microtensile bond strength (μ‐tbs) of composite bonded to hot‐pressed ceramic. The null hypothesis tested was that neither of the surface treatments (silanization or fluoric acid etching) would produce greater bond strength of composite resin to the ceramic. Materials and Methods:Four 7 × 7 × 5 mm hot‐pressed ceramic blocks of IPS Empress 2 were fabricated and polished to 600 grit followed by sandblasting with 50 μm alumina. The ceramic blocks were then divided into four groups and submitted to the following surface treatments: Group 1: 9.5% hydrofluoric (HF) acid for 20 seconds and silane (S) for 3 minutes; Group 2: silane for 3 minutes; Group 3: 9.5% HF acid for 20 seconds; Group 4: no treatment. Scotchbond adhesive was applied to the treated ceramic surfaces and covered with Filtek Z250 composite resin. The composite‐ceramic blocks were cut with an Isomet low speed diamond saw machine producing sticks (n = 25), which were loaded to failure under tension in an Instron Universal testing machine. The mean μ‐tbs was analyzed with one‐way ANOVA and Bonferroni “t” test. Results:All specimens of Group 4 experienced adhesive failure during the cutting of the block and were eliminated. The mean μ‐tbs and standard deviations (SD) in megaPascals were: Group 1 = 56.8 (±10.4), Group 2 = 44.8 (±11.6), Group 3 = 35.1 (±7.7). Statistical analysis showed that the bond strength was significantly affected by surface treatment (p < 0.0001). Group 1 (HF + S) had the highest μ‐tbs, and Group 2 (S) had higher μ‐tbs than Group 3 (HF). The mode of fracture of the specimens was examined using scanning electron microscopy (SEM), and all fractures occurred within the adhesion zone. Conclusion:The results show that surface treatment is important for resin adhesion to ceramic and suggest that silane treatment was the main factor responsible for resin bonding to ceramic.Keywords
This publication has 41 references indexed in Scilit:
- Micro-shear bond strength of dual-cured resin cement to glass ceramicsDental Materials, 2002
- In vitro dentinal surface reaction of 9.5% buffered hydrofluoric acid in repair of ceramic restorations: A scanning electron microscopic investigationThe Journal of Prosthetic Dentistry, 2000
- Effects of Treatment and Storage Conditions on Ceramic/Composite Bond StrengthJournal of Dental Research, 1995
- Relationship between surface area for adhesion and tensile bond strength — Evaluation of a micro-tensile bond testDental Materials, 1994
- Molecular Orientation of Silane at the Surface of Colloidal SilicaJournal of Dental Research, 1993
- Composition, reactivity and surface interactions of three dental silane primersDental Materials, 1993
- The influence of surface conditions and silane agents on the bond of resin to dental porcelainDental Materials, 1992
- Porcelain-composite interface microleakage with various porcelain surface treatmentsDental Materials, 1991
- A critique of bond strength measurementsJournal of Dentistry, 1989
- Shear Strength of the Composite Bond to Etched PorcelainJournal of Dental Research, 1987