Dependence of the properties of Ce-Zr-Y-La-M-O systems on synthetic conditions and on the nature of the transition metal M (Mn, Fe, Co)

Authors:

Abstract
The effects of synthetic conditions, component ratios, and the nature of the transition metal on the physicochemical and catalytic properties of Ce-Zr-Y-La-M-O (M = Mn, Fe, Co) systems are studied. The Ce-Zr-Y-La-M-O samples precipitated at ∼23°C and calcined at 600°C are single-phase and are solid solutions with a fluorite structure, which persists upon calcination at 1150°C. The Ce-Zr-Y-La-Fe(Co)-O samples precipitated at 70°C and calcined at 1150°C consist of two solid solutions, one cubic, and the other tetragonal. The specific surface area (S sp) of the samples precipitated at ∼23°C and calcined at 600°C increases in the order Ce-Zr-Y-La-O < Ce-Zr-Y-La-Mn-O < Ce-Zr-Y-La-Co-O ≈ Ce-Zr-Y-La-Fe-O. The specific surface area of the samples precipitated at 70°C is independent of M and is ∼110 m2/g. Calcination at 1150°C reduces S sp approximately by two orders of magnitude. The TPR of the unpromoted systems in H2 proceeds in two steps at 600–650 and 750–840°C. The introduction of M decreases the reduction temperatures and gives rise to a lower temperature peak between 150 and 300°C. The most effective promoter is cobalt. The fluorite-type catalysts containing no noble metal are active in NO reduction (X NO ≈ 100%) at T react = 400–450°C. The cobalt-containing catalysts are the most active in the oxidation of CO (X max = 28%) and hydrocarbons (X max = 4.3%).

This publication has 16 references indexed in Scilit: