The effect of different heat treatment cycle on hot corrosion and oxidation behavior of Ti–6Al–4V
- 1 September 2019
- journal article
- research article
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (11) , 116599
Abstract
In this paper, hot corrosion and oxidation behavior of Ti-6Al-4V alloys, which undergo different heat treatment, is investigated. For this purpose, four samples with different thermal histories were prepared by annealing, solutionizing, quenching in water and air and finally aged. The solutionizing temperature was 800 and 950°C. Also, the aging temperature was 1050°C. After the heat treatment process, the samples were exposed to a hot corrosion environment with a mixture of 60% V2O5 + 40% Na2SO4 as well as the oxidation process in the air. Microstructural and phase studies were performed by Scanning Electron Microscopy (SEM), and X-ray Diffraction (XRD), respectively, demonstrated that the samples that solution treated in 1050°C for 1 h then quenched in water and aged at 550°C for 4 h has the lowest hot corrosion and oxidation rate. Achieving maximum hot corrosion resistance without applying hot corrosion-resistant coatings can improve the durability of the parts in the petrochemical and gas turbine industries after coating or in case of coating failure.Keywords
This publication has 32 references indexed in Scilit:
- A dislocation density-based crystal plasticity constitutive model for prismatic slip in α-titaniumActa Materialia, 2011
- Effect of heat treatment on mechanical properties of Ti–6Al–4V ELI alloyMaterials Science and Engineering: A, 2009
- Oxidation of Ti–6Al–4V alloyJournal of Alloys and Compounds, 2009
- Failure analysis of Ti6Al4V gas turbine compressor bladesEngineering Failure Analysis, 2008
- A study on the hot corrosion behavior of Ti–6Al–4V alloyMaterials Letters, 2007
- Surface modification of a Ti–6Al–4V alloy by thermal oxidationSurface and Coatings Technology, 2005
- Characterization of titanium alloy Ti-6Al-4V for chemical, marine and industrial applicationsMaterials Characterization, 2003
- High-temperature corrosion of Ti and Ti-6Al-4V alloyOxidation of Metals, 1996
- Air oxidation behaviour of Ti6Al4V alloy between 650 and 850°Corrosion Science, 1994
- Material selection in the design of the femoral component of cemented total hip replacementsClinical Materials, 1986