Abstract
This study developed a hydrothermal-crystallization coupling strategy for selective titanium extraction from low-grade titanium-bearing blast furnace slag. Systematic parametric optimization revealed that an optimum titanium extraction efficiency of 92.3% was achieved under mild hydrothermal conditions. Phase evolution analysis demonstrated that the leaching residues comprised commercially valuable calcium oxalate hydrate and amorphous silica aggregates, while titanium primarily existed as stable Ti(OH)2(C2O4)22− complexes in the leachate. Subsequently, 99.4% of titanium in the leachate was precipitated through the hydrothermal decomposition method, and mixed-phase titanium oxides with a grade of 90.5% were obtained through alkaline washing. Comparative analysis highlights three notable advantages over conventional metallurgical processes: (1) selective extraction specificity for low-concentration titanium minerals, (2) process intensification through integrated hydrothermal-crystallization operations, and (3) environmental benignancy via reagent recyclability.
Funding Information
  • Science Research Project of the Hebei Education Department (QN2025372, 202305B017, CGX2024KMP1A24)
  • 2023 Annual Science and Technology Special Project for the Construction of Chengde National Innovation Demonstration Zone for Sustainable Development Agenda (QN2025372, 202305B017, CGX2024KMP1A24)
  • Chengde High-tech Industrial Development Zone Chengde HeHe co-maker space innovation and entrepreneurship project (QN2025372, 202305B017, CGX2024KMP1A24)

This publication has 28 references indexed in Scilit: