Influence of the Water Composition on the Selectivity of Apatite Flotation
- 15 February 2012
- journal article
- research article
- Published by Taylor & Francis in Separation Science and Technology
- Vol. 47 (4) , 606-612
Abstract
The effect of ionic species on the flotation selectivity of apatite was evaluated. Water containing fluoride, calcium, magnesium, and phosphate was used in the flotation experiments carried out in a flotation column for coarse and fine phosphate ore. The selectivity of apatite over ferrous and siliceous gangue was investigated. Coarse and fine ores showed different sensitivities according to the ion concentration. The results clearly showed the harmful effect of the ionic species under study on apatite selectivity. The contaminants responsible for the lowest selectivity ratios for ferrous and silicate gangue were calcium and magnesium, regardless of particle size.Keywords
This publication has 30 references indexed in Scilit:
- The flotation of fine particles using charged microbubblesMinerals Engineering, 2008
- Effects of high magnesium ion concentration on KCl flotation: Part II – Plant researchMinerals Engineering, 2007
- Multivariate projection methods applied to flotation columnsMinerals Engineering, 2005
- Influence of operating parameters on the flotation of apatiteMinerals Engineering, 2004
- Reagents used in the flotation of phosphate ores: a critical reviewMinerals Engineering, 2003
- Effect of calcium ions and citric acid on the flotation separation of chalcopyrite from galena using dextrinMinerals Engineering, 2000
- Effect of particle size on flotation performance of complex sulphide oresMinerals Engineering, 1999
- Interfering ions in the flotation of a phosphate ore in a batch columnMinerals Engineering, 1999
- Troubleshooting industrial flotation columnsMinerals Engineering, 1995
- A review of water re-use in flotationMinerals Engineering, 1989