Chemical, Mechanical and Tribological Effects of Artificially Aging up to 6 Weeks on Virgin and Crosslinked UHMWPE Evaluated for a TKR Design
Open Access
- 24 July 2025
- journal article
- research article
- Published by MDPI AG in Bioengineering
- Vol. 12 (8) , 793
Abstract
Patients undergo total knee arthroplasty (TKA) at younger ages with the expectation that the devices will perform well over two to three decades. During this time, the ultra-high molecular weight polyethylene (UHMWPE) bearing material properties of the implant may change due to aging induced by radiation and oxygen diffusion or other effects. Vitamin E or other antioxidants are promoted since several years to improve the oxidation resistance of UHMWPE. To compare the effectivity of these substances against established materials, a six weeks aging process was used and the chemical, mechanical and bio-tribological properties were analysed. Highly crosslinked and two weeks aged UHMWPE served as a reference for the currently established aging standards and virgin UHMWPE was aged for six weeks to separate the effects of crosslinking and vitamin E blending. Six weeks artificially aging changed the chemical, mechanical and bio-tribological properties of cross-linked UHMWPE significantly compared to only two weeks artificially aging, leading to cracks and delamination during the highly demanding activities wear test. The degradative effect of extended aging was also observed for virgin UHMWPE. These observations are in good accordance to retrieval findings. Minor changes on the chemical properties were observed for the cross-linked UHWMPE blended with vitamin E without impact on the mechanical and bio-tribological properties.Keywords
This publication has 152 references indexed in Scilit:
- In vitro wear performance of standard, crosslinked, and vitamin‐E‐blended UHMWPEJournal of Biomedical Materials Research Part A, 2011
- Trace concentrations of vitamin E protect radiation crosslinked UHMWPE from oxidative degradationJournal of Biomedical Materials Research Part A, 2008
- Accelerated aging studies of UHMWPE. II. Virgin UHMWPE is not immune to oxidative degradationJournal of Biomedical Materials Research, 2002
- Accelerated aging studies of UHMWPE. I. Effect of resin, processing, and radiation environment on resistance to mechanical degradationJournal of Biomedical Materials Research, 2002
- Identification and quantification of irradiation in UHMWPE throughtrans-vinylene yieldJournal of Biomedical Materials Research, 2001
- Comparison of three joint simulator wear debris isolation techniques: Acid digestion, base digestion, and enzyme cleavageJournal of Biomedical Materials Research, 2001
- Evaluation of the response of primary human peripheral blood mononuclear phagocytes to challenge within vitro generated clinically relevant UHMWPE particles of known size and doseJournal of Biomedical Materials Research, 2000
- Quantitative analysis of ultrahigh molecular weight polyethylene (UHMWPE) wear debris associated with total knee replacementsJournal of Biomedical Materials Research, 2000
- A miniature specimen mechanical testing technique scaled to articulating surface of polyethylene components for total joint arthroplastyJournal of Biomedical Materials Research, 1999
- Component wear of total knee prostheses using Ti‐6Al‐4V, titanium nitride coated Ti‐6Al‐4V, and cobalt‐chromium‐molybdenum femoral componentsJournal of Biomedical Materials Research, 1988