Effect of firing protocols on cohesive failure of all-ceramic crowns
Authors:
- Elke KrögerEKElke Kröger
- Denise MüllerDMDenise Müller
- Marc SchmitterMSMarc Schmitter
- 1 December 2010
- journal article
- Published by Elsevier in Journal of Dentistry
- Vol. 38 (12) , 987-994
Abstract
No abstract availableKeywords
This publication has 14 references indexed in Scilit:
- Reliability of Metalloceramic and Zirconia-based Ceramic CrownsJournal of Dental Research, 2010
- Clinical performance of extended zirconia frameworks for fixed dental prostheses: two‐year resultsJournal of Oral Rehabilitation, 2009
- High-strength CAD/CAM-fabricated veneering material sintered to zirconia copings — A new fabrication mode for all-ceramic restorationsDental Materials, 2009
- A systematic review of the survival and complication rates of all‐ceramic and metal–ceramic reconstructions after an observation period of at least 3 years. Part II: fixed dental prostheses.Clinical Oral Implants Research, 2007
- Load‐bearing capacity of all‐ceramic posterior four‐unit fixed partial dentures with different zirconia frameworksEuropean Journal of Oral Sciences, 2007
- Fatigue of zirconia under cyclic loading in water and its implications for the design of dental bridgesDental Materials, 2007
- All‐ceramic fixed partial dentures designed according to the DC‐Zirkon® technique. A 2‐year clinical studyJournal of Oral Rehabilitation, 2005
- Strength, reliability and mode of fracture of bilayered porcelain/zirconia (Y-TZP) dental ceramicsBiomaterials, 2004
- Shear strength of core-veneer interface in bi-layered ceramicsThe Journal of Prosthetic Dentistry, 2004
- The influence of the veneering porcelain and different surface treatments on the biaxial flexural strength of a heat-pressed ceramicThe Journal of Prosthetic Dentistry, 2003