(Ti, O)/Ti and (Ti, O, N)/Ti composite coatings fabricated via PIIID for the medical application of NiTi shape memory alloy
Authors:
- 22 November 2010
- journal article
- research article
- Published by Wiley in Journal of Biomedical Materials Research Part B: Applied Biomaterials
- Vol. 96B (2) , 249-260
Abstract
In this investigation, the plasma immersion ion implantation and deposition (PIIID) technique was used to fabricate (Ti, O)/Ti or (Ti, O, N)/Ti coatings on a NiTi shape memory alloy (SMA, 50.8 at.% Ni) to improve its corrosion, wear resistance, and bioactivity. After coating fabrication, the structure and properties of composite coatings were studied, and the coated and uncoated NiTi SMA samples were compared with each other. Scanning electron microscopic (SEM) examination of coating surfaces and cross‐sections showed that (Ti, O)/Ti and (Ti, O, N)/Ti composite coatings were dense and uniform, having thickness values of 1.16 ± 0.08 μm and 0.95 ± 0.06 μm, respectively. X‐ray diffraction (XRD) results revealed that there were no diffraction peaks corresponding to TiO2 or TiN for (Ti, O)/Ti and (Ti, O, N)/Ti composite coatings, suggesting that after the PIIID treatment, TiO2 and TiN were amorphous or nanosized in the coatings. Energy dispersive X‐ray (EDX) analysis indicated that the interface between the coating and NiTi SMA substrate was gradual rather than sharp. In addition, EDX elemental mapping of coating cross‐sections showed that Ni was depleted from the surface. Differential scanning calorimetry (DSC) curves revealed that the shape memory ability of NiTi SMA was not degraded by the PIIID treatment. The width of wear tracks on (Ti, O, N)/Ti coated NiTi SMA samples was reduced 6.5‐fold, in comparison with that on uncoated samples. The corrosion potential (Ecorr) was improved from −466.20 ± 37.82 mV for uncoated samples to 125.50 ± 21.49 mV and −185.40 ± 37.05 mV for (Ti, O)/Ti coated and (Ti, O, N)/Ti coated samples, respectively. Both types of coatings facilitated bone‐like apatite formation on the surface of NiTi SMA in simulated body fluid (SBF), indicating their in vitro bioactivity. © 2010 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 2011.Keywords
This publication has 30 references indexed in Scilit:
- A comparative study on titania layers formed on Ti, Ti-6Al-4V and NiTi shape memory alloy through a low temperature oxidation processSurface and Coatings Technology, 2010
- Blood compatibilities of carbon nitride film deposited on biomedical NiTi alloyDiamond and Related Materials, 2009
- Ti based biomaterials, the ultimate choice for orthopaedic implants – A reviewProgress in Materials Science, 2009
- Fabrication of an Apatite/Collagen Composite Coating on the NiTi Shape Memory Alloy through Electrochemical Deposition and Coating CharacterisationMaterials Science Forum, 2009
- Low-temperature biomimetic formation of apatite/TiO2 composite coatings on Ti and NiTi shape memory alloy and their characterizationApplied Surface Science, 2008
- Pseudotumours associated with metal-on-metal hip resurfacingsThe Journal of Bone and Joint Surgery. British volume, 2008
- Influence of nickel ions on human multipotent mesenchymal stromal cells (hMSCs)Materialwissenschaft und Werkstofftechnik, 2007
- TiN/ZrO2 multilayers synthesized on GCr15 bearing steel using plasma immersion ion implantation and depositionSurface and Coatings Technology, 2007
- New oxidation treatment of NiTi shape memory alloys to obtain Ni‐free surfaces and to improve biocompatibilityJournal of Biomedical Materials Research Part B: Applied Biomaterials, 2005
- Nickel essentiality, toxicity, and carcinogenicityCritical Reviews in Oncology/Hematology, 2002