Influence of grain size on wear behavior of SiC coating for carbon/carbon composites at elevated temperatures
Authors:
- Zishan ChenZCZishan Chen
- Hejun LiHLHejun Li
- Kezhi LiKLKezhi Li
- Qingliang ShenQSQingliang Shen
- Qiangang FuQFQiangang Fu
- 1 January 2014
- journal article
- Published by Elsevier in Materials & Design (1980-2015)
- Vol. 53, 412-418
Abstract
No abstract availableKeywords
This publication has 27 references indexed in Scilit:
- The preparation and mechanical properties of carbon–carbon/lithium–aluminum–silicate composite jointsMaterials & Design (1980-2015), 2013
- Wear-mechanical properties of filler-added liquid silicon infiltration C/C–SiC compositesMaterials & Design (1980-2015), 2013
- Simulated three-dimensional transient temperature field during aircraft braking for C/SiC composite brake discMaterials & Design (1980-2015), 2011
- Real-time damage evaluation of a SiC coated carbon/carbon composite under cyclic fatigue at high temperature in an oxidizing atmosphereMaterials Science and Engineering: A, 2009
- Silicon carbide coating to protect carbon/carbon composites against oxidationScripta Materialia, 2005
- Tribological behavior of ceramic materials (Si 3 N 4 , SiC and Al 2 O 3 ) in aqueous mediumJournal of the European Ceramic Society, 2004
- Oxidation resistant carbon materials derived from boronated carbon–silicon alloysCarbon, 2004
- Influence of the preparation temperature on the phase, microstructure and anti-oxidation property of a SiC coating for C/C compositesCarbon, 2004
- On temperature-dependent tribological regimes and oxidation of carbon-carbon composites up to 1800°CWear, 1996
- Tribological Characteristics of SiC Ceramics in High‐Temperature and High‐Pressure WaterJournal of the American Ceramic Society, 1994