Growth of a W/TiN-bilayer coating: an alternative to diffusion barrier keeping the hard coating condition of the system
Authors:
- Amilkar FragielAFAmilkar Fragiel
- Francisco Solis-PomarFSFrancisco Solis-Pomar
- Abel FundoraAFAbel Fundora
- Bernardo CampilloBCBernardo Campillo
- José María Malo-TamayoJMJosé María Malo-Tamayo
- Ana María Campos-ChinchillaACAna María Campos-Chinchilla
- Aly Castellanos-SuárezACAly Castellanos-Suárez
- Mercedes Teresita Oropeza-GuzmánMOMercedes Teresita Oropeza-Guzmán
- Eduardo Perez-TijerinaEPEduardo Perez-Tijerina
Open Access
- 2 January 2026
- journal article
- Published by International Association of Physical Chemists (IAPC) in Journal of Electrochemical Science and Engineering
- Vol. 16, 2983
Abstract
An evaluation of the improvement provided by a W thin film, when incorporated into a TiN bilayer coating system on 304 stainless steel, is reported after determining its electrochemical behaviour and mechanical properties. The TiN-bilayer and W/TiN-bilayer coatings were prepared by balanced magnetron sputtering. Coating structure, morphology, interphase, and chemical composition were determined by scanning electron microscopy, Auger electron spectroscopy and X-ray diffraction. Mechanical properties were determined by the nanoindentation technique. The electrochemical behavior was investigated by electrochemical impedance spectroscopy (EIS) using 6 wt.% NaCl solution as electrolyte. The electrochemical results showed an increase in overall corrosion resistance (Rp) when the W thin film is incorporated into the TiN-bilayer coating system. The Rp for the initial measurement is 187.6 and 347.9 kΩ cm2 for the TiN-bilayer coating system and W/TiN-bilayer coating system, respectively. The results obtained from the EIS study over time indicate that the Rp after 7 weeks of immersion are 53.2 and 119.8 kΩ cm2 for the TiN-bilayer coating system and W/TiN-bilayer coating system, respectively. Nanoindentation hardness measurements showed a slight difference between the two coating systems. The TiN-bilayer hardness showed a value of approximately 24 GPa, while the W/TiN-bilayer hardness showed a value of approximately 22 GPa. Considering other beneficial properties associated with W, the results showed that a W/TiN-bilayer coating system can be used as an alternative hard and protective coating system on steel substrates to mitigate corrosion damage.Keywords
Funding Information
- Fondo Nacional de Ciencia Tecnología e Innovación (2022OPGP39)
This publication has 44 references indexed in Scilit:
- Pyramidal structure that promotes the photothermal effects of TiN films for de-icing applicationsCeramics International, 2025
- Highly Oriented Zirconium Nitride and Oxynitride Coatings Deposited via High‐Power Impulse Magnetron Sputtering: Crystal‐Facet‐Driven Corrosion Behavior in Domestic WastewaterAdvanced Engineering Materials, 2021
- Enhancement in corrosion resistance and vibration damping performance in titanium by titanium nitride coatingSN Applied Sciences, 2020
- Blistering of tungsten films deposited by magnetron sputtering after helium irradiationFusion Engineering and Design, 2018
- Experimental studies of the effect of Ti interlayers on the corrosion resistance of TiN PVD coatings by using electrochemical methodsCorrosion Science, 2018
- Corrosion mechanism in PVD deposited nano-scale titanium nitride thin film with intercalated titanium for protecting the surface of siliconElectrochimica Acta, 2018
- Structural characterizations of magnetron sputtered nanocrystalline TiN thin filmsMaterials Characterization, 2008
- Correlation between optical characterization of the plasma in reactive magnetron sputtering deposition of Zr–N on SS 316L and surface and mechanical properties of the deposited filmsApplied Surface Science, 2008
- Relationship between Condition of Deposition and Properties of W‐Ti‐N Thin Films Prepared by Reactive Magnetron SputteringAdvanced Engineering Materials, 2006
- Hardness measurements of thin filmsThin Solid Films, 1984