Surface degradation evaluation of different self‐adhesive restorative materials after prolonged energy drinks exposure
Author:
- 12 August 2020
- journal article
- research article
- Published by Wiley in Journal of Esthetic and Restorative Dentistry
- Vol. 32 (7) , 707-714
Abstract
Aim: To evaluate the effects of energy drinks and soft beverages on the surface degradation of different self‐adhesive materials.Materials and methods: A 156 disc shaped specimens of each of the following materials were prepared: Alkasite (Cention N, CN), High viscozity glass ionomer (Equia Forte, EF), Glass Carbomer (GCP Fill, GC) (n = 52). After specimen preparations, baseline surface roughness measurements were done using a 3D non‐contact optical profilometer. Then, specimens were subdivided into 4 subgroups (n = 13) and stored in petri dish containing Red Bull; Burn; Coca‐Cola and Distilled water. The surface roughness of the specimens were measured after 1‐day, 1‐week, and 1‐month of immersion in beverages.Result: It was observed that 1‐month Red Bull immersion revealed the highest roughness difference (ΔRa) for each self‐adhesive restorative material and this was followed by Burn. Whereas, the lowest ΔRa values were observed after 1‐day coke and distilled water immersion in all tested material groups (P < 0.05). Coke and distilled water presented the energy drinks' 1‐day immersion affect, after 1‐week immersion (P < 0.05).Conclusion: The energy drinks have a substantially damaging effect on roughness of self adhesive materials compared with soft drinks and distilled water; and this effect is increasing with exposure duration.Keywords
This publication has 27 references indexed in Scilit:
- Characterisation of a remineralising Glass Carbomer® ionomer cement by MAS-NMR SpectroscopyDental Materials, 2012
- Acids with an equivalent taste lead to different erosion of human dental enamelDental Materials, 2011
- In Vitro Evaluation of Surface Roughness and Microhardness of Restorative Materials Submitted to Erosive ChallengesOperative Dentistry, 2011
- Effects of Various Beverages on Hardness, Roughness, and Solubility of Esthetic Restorative MaterialsJournal of Esthetic and Restorative Dentistry, 2011
- Health Effects of Energy Drinks on Children, Adolescents, and Young AdultsPediatrics, 2011
- Short Communication: In vitro assessment of Erosive Potential of Energy DrinksEuropean Archives of Paediatric Dentistry, 2010
- Properties and modification of soft drinks in relation to their erosive potential in vitroJournal of Dentistry, 2005
- Influence of food-simulating solutions and surface finish on susceptibility to staining of aesthetic restorative materialsJournal of Dentistry, 2005
- In vitro Quantitative Assessment of Enamel Microhardness after Exposure to Eroding Immersion in a Cola DrinkCaries Research, 1998
- The Mechanism for Erosion of Glass-ionomer Cements in Organic-Acid Buffer SolutionsJournal of Dental Research, 1990