Tensile Properties of the Subsurface and Center Regions of AA6111 Direct-Chill-Cast Ingot in Semisolid State and Their Hot Tearing Susceptibility
Open Access
- 12 September 2023
- conference paper
- Published by MDPI AG in Engineering Proceedings
- Vol. 43 (1) , 9
Abstract
AA6111 alloys are widely used in the automotive industry owing to their high strength/weight ratio, good corrosion resistance, and reasonable formability. During their manufacture through ingot metallurgy via direct chill (DC) casting, the alloys often suffer from hot tearing, limiting DC casting productivity. The present study focused on evaluating the mechanical properties in the semisolid state and the hot tearing susceptibility of AA6111 DC-cast ingot in the subsurface and center regions. The mechanical behavior of two different regions at high temperatures above solidus was studied using smoothed and notched samples. Tensile tests were performed using the Gleeble 3800 thermomechanical testing unit, and the digital image correlation method was applied to measure the strain evolution. The change in the grain structure in the subsurface and the presence of a high-volume fraction of needle-like β-Fe intermetallics significantly reduced the ductility of the cast ingot in the subsurface region. The hot tearing susceptibility in the subsurface region of the cast ingot was higher than that in the center region. The notch effect is more significant in the subsurface on the stress sensitivity in the presence of stress raisers compared with that in the center region.Keywords
Funding Information
- The Natural Sciences and Engineering Research Council of Canada (NSERC) (CRDPJ 514651-17, 2018-LU-252831, IT14722)
- Fonds de Recherche du Quebec-Nature et Technologies (FRQNT) (CRDPJ 514651-17, 2018-LU-252831, IT14722)
- the Mitacs Acceleration (CRDPJ 514651-17, 2018-LU-252831, IT14722)
This publication has 21 references indexed in Scilit:
- Hot Tearing in Al-Mg-Si Alloys with Minor Additions of Cu or MnMaterials Science Forum, 2011
- Assessment of High-Temperature Brittleness Range of the Casted Alloy AZ91Materials Science Forum, 2011
- Macrosegregation in direct-chill casting of aluminium alloysProgress in Materials Science, 2008
- Structure observations related to hot tearing of Al–Cu billets produced by direct-chill castingMaterials Science and Engineering: A, 2006
- Rheological behavior of Al-Cu alloys during solidification constitutive modeling, experimental identification, and numerical studyMetallurgical and Materials Transactions A, 2005
- The use of water cooling during the continuous casting of steel and aluminum alloysMetallurgical and Materials Transactions A, 2005
- Structure formation and macrosegregation under different process conditions during DC castingMaterials Science and Engineering: A, 2004
- Mechanical properties in the semi-solid state and hot tearing of aluminium alloysProgress in Materials Science, 2004
- Texture control by thermomechanical processing of AA6xxx Al–Mg–Si sheet alloys for automotive applications—a reviewMaterials Science and Engineering: A, 2002
- Growth related metastable phase selection in a 6xxx series wrought Al alloyMaterials Science and Engineering: A, 2001