Fabrication and magnetic properties of Co0.05LaTi0.95O3 nanofibers

Authors:

Abstract
Co0.05LaTi0.95O3 nanofibers with average diameter of 201 – 264 nm have been successfully fabricated by electrospinning method. The crystal structure of nanofibers calcined at 400 – 700 °C shows amorphous structure. The Co0.05LaTi0.95O3 nanofibers calcined at 800 °C had cubic perovskite-type structure with secondary phase. The average crystallite sizes of nanofibers calculated from Scherrer's formula were found to be 8.6 nm. The nanofibers of Co0.05LaTi0.95O3 calcined at 400 – 600 °C exhibit diamagnetic properties. The sample of nanofibers calcined at 700 and 800 °C revealed room-temperature ferromagnetism behavior with the highest magnetization of 2.6 emu/g observed in the sample calcined at 800 °C. It was found that the magnetization value increased with increasing calcination temperature.

This publication has 16 references indexed in Scilit: