The effect of nitriding on adhesion and mechanical properties of electroless Ni–P coating on AISI 4140 steel
- 1 February 2017
- journal article
- research article
- Published by SAGE Publications in Surface Engineering
- Vol. 33 (2) , 116-121
Abstract
In this work, electroless nickel has been deposited onto steel substrates by a selfcatalytic process, which involves temperature and time to create a Ni–P layer with a uniform thickness. The major drawback of electroless nickel is the interdiffusion post heat treatment (PHT) that is necessary to create a metallurgical bond between the steel substrate and the Ni–P deposit. The PHT results in softening of the steel. The aim of this ongoing research is to investigate the effect of introducing a nitrided layer prior to deposition of Ni–P layer, as an attempt to lessen the softening of the steel. To this end, Ni–P coatings were obtained over nitrided and non-nitrided steel substrates. The PHT was done at 400°C or 610°C. The nitrided layer, indeed, avoided the softening of the steel substrate. In addition, the nitrided layer improves the adhesion of the Ni–P coating even when the PHT was done at 400°C.Keywords
Funding Information
- FINEP and CNPq (01.10.0634)
- FINEP and CNPq (01.10.0634)
This publication has 18 references indexed in Scilit:
- Hardness and structural correlation for electroless Ni alloy depositsJournal of Materials Science, 2007
- Effect of accelerators and stabilizers on the formation and characteristics of electroless Ni–P depositsMaterials Chemistry and Physics, 2006
- An overall aspect of electroless Ni-P depositions—A review articleMetallurgical and Materials Transactions A, 2006
- Deposition of electroless Ni–P graded coatings and evaluation of their corrosion resistanceSurface and Coatings Technology, 2006
- Hardness evolution of electroless nickel–phosphorus deposits with thermal processingSurface and Coatings Technology, 2003
- The tribological characteristics of electroless NiP coatingsWear, 2001
- Fatigue properties of an AISI 1045 steel coated with an electroless Ni-P depositThin Solid Films, 1999
- Effect of the thickness of an electroless Ni–P deposit on the mechanical properties of an AISI 1045 plain carbon steelSurface and Coatings Technology, 1998
- Influence of electroless Ni-P deposits on the corrosion-fatigue properties of an AISI 1045 steelThin Solid Films, 1997
- Influence of NiP electroless coating on the fatigue behavior of plain carbon steelsThin Solid Films, 1996