Fabrication of a lotus-type porous Al-Si alloy by continuous casting with a thermal decomposition method
Open Access
- 1 May 2009
- conference paper
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 165 (1) , 012067
Abstract
Lotus-type porous A1-14 wt.%Si alloy was fabricated by continuous casting at a transference velocity of 10 mmmin-1 in vacuum and by adding Ca(OH)2 pellets to the crucible. The porosity and the pore diameter increased by varying the amount of Ca(OH)2 from 0.2 g to 0.6 g. In the case of 0.6 g Ca(OH)2, the average porosity was about 30 % and the average pore diameter was about 3.8 mm. XRD patterns of the pellets after continuous casting showed the Ca(OH)2 pellet did not decompose completely during continuous casting. The TG-DTA analysis showed that the Ca(OH)2 pellet decomposes more slowly than Ca(OH)2 powder. These results suggest that the Ca(OH)2 pellets gradually decomposed in the crucible during the continuous casting, which is suitable for the supply of hydrogen over extended periods.Keywords
This publication has 5 references indexed in Scilit:
- Fabrication of Porous Copper with Directional Pores through Thermal Decomposition of CompoundsMetallurgical and Materials Transactions A, 2008
- Fabrication, properties and application of porous metals with directional poresProgress in Materials Science, 2007
- Anisotropic mechanical properties of porous copper fabricated by unidirectional solidificationMaterials Science and Engineering: A, 2001
- Manufacture, characterisation and application of cellular metals and metal foamsProgress in Materials Science, 2001
- Thermal decomposition of calcium hydroxide deposited on the substrateThermochimica Acta, 1994