Corrosion Analysis of Orthodontic Wires: An Interaction Study of Wire Type, pH and Immersion Time

Authors:

Abstract
Variety of metal alloy wires are used in modern orthodontic treatment, such as, Stainless Steel (SS), cobalt-chromium, Nickel-Titanium (NiTi), Beta-Titanium (TMA), etc. These metal alloy wires are subjected to biodegradation in oral environments leading to corrosion. Although the risk is low, corrosion products such as nickel and chromium may cause sensitivities or allergic reactions during orthodontic treatment [1-5]. Other consequences may involve discoloration or roughening of surface leading to friction between the bracket and the arch wire [1,2]. Several intrinsic and environmental factors influence the corrosion reactions of orthodontic wires such as, types of alloys, surface roughness, surface coating, electrolyte, pH value, aging, immersion time and temperature [1,3,4,6-12].