Hydrogen concentration limit and critical temperatures for delayed hydride cracking in zirconium alloys
Authors:
- S.-Q. ShiSSS.-Q. Shi
- G.K. ShekGSG.K. Shek
- M.P. PulsMPM.P. Puls
- 1 February 1995
- journal article
- Published by Elsevier in Journal of Nuclear Materials
- Vol. 218 (2) , 189-201
Abstract
No abstract availableKeywords
This publication has 12 references indexed in Scilit:
- The hydrostatic stress field around the crack tip in zirconium 2.5% niobium and implications for delayed hydride crackingScripta Metallurgica et Materialia, 1991
- Effects of crack tip stress states and hydride-matrix interaction stresses on delayed hydride crackingMetallurgical Transactions A, 1990
- High temperature limit for delayed hydride crackingScripta Metallurgica, 1988
- The nucleation of hydrides in a Zr-2.5 wt% Nb alloyJournal of Nuclear Materials, 1984
- The form of crack tip plastic zonesEngineering Fracture Mechanics, 1984
- Solubility of hydrogen isotopes in stressed hydride-forming metalsScripta Metallurgica, 1983
- On the existence of a memoty effect in hydride precipitation in cold-worked Zr-2.5% NbJournal of Nuclear Materials, 1977
- Singular behaviour at the end of a tensile crack in a hardening materialJournal of the Mechanics and Physics of Solids, 1968
- Plane strain deformation near a crack tip in a power-law hardening materialJournal of the Mechanics and Physics of Solids, 1968
- The Thermodynamics of Stressed SolidsZeitschrift für Physikalische Chemie, 1966