Bifilm defects in ductile-iron support bracket castings
Authors:
- 21 December 2016
- journal article
- research article
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 30 (3) , 148-158
Abstract
Many filling defects such as bi-film defect, gas bubble, loosed sand and etc., are developed by turbulent filling. These defects entrapped and flowed along mold cavity during the filling process. As a result, they makes casting property unreliable and unpredictable. The best way to prevent the filling defect is to control the gating velocity under a critical value using a bottom gating runner system. Two different gating system, top- and bottom- systems, are applied for casting ductile-iron support bracket. For these two runner systems, their filling defects are predicted by a numerical modeling. Two- and three- parameter Weibull probability are plotted to analyze the reliabilities of the mechanical properties of the castings from these two gating systems. A good and reliable runner system for casting a high elongation and fracture toughness of the support bracket was proposed in this study.Keywords
This publication has 6 references indexed in Scilit:
- Confluence weld in an aluminum gravity castingJournal of Materials Processing Technology, 2012
- Foam Filters Used in Gravity CastingMetallurgical and Materials Transactions B, 2011
- Shape Casting2011
- Weibull Analysis of Mechanical Data for Castings: A Guide to the Interpretation of Probability PlotsMetallurgical and Materials Transactions A, 2010
- Quality Indices for Aluminum Alloy Castings: A Critical ReviewMetallurgical and Materials Transactions B, 2009
- Statistical distributions of fracture strengths of cast Al7SiMg alloyMaterials Science and Engineering: A, 1993