Abstract
Solid-state hydrogen storage offers high volumetric density and low operating pressure. Hydrogen is flammable, and its leakage could lead to fire or explosion hazards. Unlike the rapid release of gaseous hydrogen, solid-state storage materials may release hydrogen for several minutes continuously, providing a time window for inhibition. In this study, a water-interference desorption apparatus was developed to investigate water-induced inhibition of accidental hydrogen release from LaNi5 alloy. The effects of water interference on desorption behavior, and the recovery of hydrogen absorption and desorption performance after water interference were tested at 0, 10, 20 and 30 °C. The results show that, at 20 °C, water interference reduces the hydrogen desorption volume to 85.7% of that without interference, increases the desorption completion time to 14.4 times, and decreases the average desorption rate to 5.9%. Further risk assessment based on the Gaussian puff model shows substantial reductions in the peak hydrogen volume fraction and the duration above the 4% hazardous concentration, and the hydrogen concentration-time integral is reduced by 95.2-95.8%. At 0, 10 and 30 °C, water interference similarly reduces the average desorption rate to 2.0-5.6% and extends the desorption time to 15.9-23.9 times. After reactivation, the hydrogen absorption and desorption performance recovers to more than 84% of the original level. These results demonstrate that water interference can substantially inhibit accidental hydrogen release and reduce the associated hydrogen leakage risk while maintaining recoverable hydrogen storage performance.

This publication has 20 references indexed in Scilit: