The curing of novolacs with paraformaldehyde
Authors:
- 1 March 1982
- journal article
- research article
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 27 (3) , 893-901
Abstract
The curing of novolacs with paraformaldehyde is analyzed with several experimental techniques (DSC, IR, sol fraction) as well as statistical arguments. Results for typical novolacs show that a maximum crosslinking density is attained at a mass ratio mP/mN close to 0.20. However, at mP/mN greater than 0.10, hemiformals appear in the cured product, increasing the amount of extractable formaldehyde. The heat of reaction increases linearly from mP/mN = 0 to 0.15, attaining a maximum value of −ΔH = 98 cal/g novolac at mP/mN ∼ 0.20. The curing kinetics follows an overall second‐order law with an activation energy E = 32.5 kcal/mol and a preexponential factor A = 1.1 × 1015 min−1 (both for mP/mN > 0.1).Keywords
This publication has 6 references indexed in Scilit:
- Novolacs from paraformaldehydeJournal of Applied Polymer Science, 1979
- A New Derivation of Average Molecular Weights of Nonlinear PolymersMacromolecules, 1976
- Determination of kinetic parameters for the reaction between phenol and formaldehyde by differential scanning calorimetryEuropean Polymer Journal, 1974
- Formation and cure of novolacs: NMR study of transient moleculesJournal of Polymer Science: Polymer Chemistry Edition, 1973
- Base‐catalyzed hydroxymethylation of phenol by aqueous formaldehyde. Kinetics and mechanismJournal of Polymer Science Part A-1: Polymer Chemistry, 1968
- Determination of rates of thermal decomposition of polymerization initiators with a differential scanning calorimeterJournal of Applied Polymer Science, 1967