Fluoride-Releasing Restorative Materials: The Effect of a Resinous Coat on Ion Release
Authors:
- Katarina KelićKKKatarina Kelić
- Matej ParMatej Par
- Kristina PerošKPKristina Peroš
- Ivana ŠutejIŠIvana Šutej
- Zrinka TarleZTZrinka Tarle
Open Access
- 15 December 2020
- journal article
- research article
- Published by University of Zagreb School of Dental Medicine in Acta Stomatologica Croatica
- Vol. 54 (4) , 371-381
Abstract
Objective: To determine the effect of two adhesive systems and a glass ionomer coating resin on fluoride release and concurrent pH changes over a period of 168 days. Material and methods: Four restorative materials were investigated: a giomer Beautiful II, an “alkasite” material Cention, a conventional composite Filtek Z250, and a glass ionomer cement Fuji IX Extra. Light-cured composite specimens were coated using G-aenial Bond and Clearfil Universal Bond Quick. Glass ionomer specimens were coated using GC Fuji Coat LC. Uncoated specimens were used as references. Quantitative fluoride release and pH changes were measured after 1 h, 24 h, 2 days, 7 days, 28 days, 84 days, and 168 days. Results: The cumulative fluoride release after 168 days increased for uncoated specimens in the following order: Filtek Z250 < Beautifil II < Cention < Fuji IX Extra. A comparatively lower fluoride release was measured for the composites coated with Clearfil Universal Bond Quick, with cumulative values after 168 days increasing in the following order: Filtek Z250 < Beautifil II < Cention. The composites coated with G-aenial Bond showed lower fluoride release compared to the uncoated specimens, with cumulative values increasing in the following order: Filtek Z250 < Beautifil II < Cention. The composites coated with G-aenial Bond showed pH values in the acidic range (4.4- 5.7) after 1 h and 24 h. Conclusion: Fluoride release varied among the investigated restorative materials and depended on the use of dental adhesives and coatings. The pH of all materials, coating types and time points varied.Keywords
This publication has 43 references indexed in Scilit:
- Long-Term Fluoride Exchanges at Restoration Surfaces and Effects on Surface Mechanical PropertiesISRN Dentistry, 2013
- Fluoride Release From a New Glass-ionomer CementOperative Dentistry, 2011
- Estimation of Fluoride Release from Various Dental Materials in Different Media—An In Vitro StudyInternational Journal of Clinical Pediatric Dentistry, 2009
- Water sorption/solubility of dental adhesive resinsDental Materials, 2006
- Effect of coinitiator and water on the photoreactivity and photopolymerization of HEMA/camphoquinone‐based reactant mixturesJournal of Biomedical Materials Research Part A, 2006
- Degree of conversion and permeability of dental adhesivesEuropean Journal of Oral Sciences, 2005
- Effects of resin hydrophilicity on water sorption and changes in modulus of elasticityBiomaterials, 2005
- Effect of resin hydrophilicity and water storage on resin strengthBiomaterials, 2004
- Adhesive phase separation at the dentin interface under wet bonding conditionsJournal of Biomedical Materials Research, 2002
- Fluoride release from glass ionomer cements and resin composites coated with a dentin adhesiveDental Materials, 2000