Extended defects formed by high-fluence helium implantation in silicon have been studied as a function of the implantation temperature, from room temperature up to 800 °C. Transmission electron microscopy results show that the formation of cavities created by a 50 keV He implantation with a fluence of can be divided into three stages. For implantation temperature up to about 300 °C the bubble size is relatively constant but the bubble density decreases due to the increase in dynamic annealing. Above 300 °C, where divacancies are no longer stable and when the helium is mobile, both the density and size of the cavities stay relatively constant. In this stage, helium starts to diffuse out and the cavities become more and more faceted as the temperature increases. Concurrently interstitial-type defects appear: small elongated rod-like defects at relatively low temperatures and large ribbon-like defects at 600 °C. Finally, for implantation at 800 °C, no cavities are formed and only dislocation loops and {113}’s (ribbon-like defects and rod-like defects), are observed depending on the deposited energy profile. At this temperature the defect annealing during implantation becomes efficient to convert ribbon-like defects into dislocation loops.
Keywords
This publication has 17 references indexed in Scilit:
- Radiation damage in He implanted silicon at high temperature using multi-energiesNuclear Instruments and Methods in Physics Research Section B: Beam Interactions with Materials and Atoms, 2002
- The effects of implantation temperature on He bubble formation in siliconNuclear Instruments and Methods in Physics Research Section B: Beam Interactions with Materials and Atoms, 2001
- Effect of implant temperature on secondary defects created by MeV Sn implantation in siliconJournal of Applied Physics, 2001
- Thermal evolution of extended defects in implanted Si:Materials Science in Semiconductor Processing, 2000
- Voids in Silicon by He Implantation: From Basic to ApplicationsJournal of Materials Research, 2000
- He-induced cavity formation in silicon upon high-temperature implantationNuclear Instruments and Methods in Physics Research Section B: Beam Interactions with Materials and Atoms, 2000
- He-vacancy interactions in Si and their influence on bubble formation and evolutionPhysical Review B, 2000
- Helium desorption/permeation from bubbles in silicon: A novel method of void productionNuclear Instruments and Methods in Physics Research Section B: Beam Interactions with Materials and Atoms, 1987
- Defects in electron-irradiated germaniumPhilosophical Magazine, 1976
- On the permeation of hydrogen and helium in single crystal silicon and germanium at elevated temperaturesPhysica, 1956