Abstract
This study examines how additions of Si, Al, Cu, and Cr powders to the stoichiometric 3Ti–Si–2C (at. %) charge influen­ce the formation of the Ti 3 SiC 2 MAX phase during self-propagating high-temperature synthesis (SHS) performed in air within a sand bed, without a sealed reactor or controlled atmosphere. The effect of partially or fully substituting elemental Ti and Si powders with TiSi 2 on the Ti 3 SiC 2 yield is also assessed. Microstructural characterization of the SHS products was conducted using scanning electron microscopy equipped with energy-dispersive spectroscopy, and the phase composition was quantified by X -ray diffraction. An addition of 0.1 mol Si to the stoichiometric mixture increases the Ti 3 SiC 2 content in the product to approximately 70 vol. %. Incorporating 0.1 mol Al decreases the Ti 3 SiC 2 fraction to 39 vol. % and results in the formation of TiAl. In contrast, combining a silicon excess with 0.1 mol Al in the 3Ti–1.25Si–2C + 0.1Al system markedly enhances the Ti 3 SiC 2 yield, reaching ~89 vol. %. For synthesis in the TiSi 2 –C system, the share of the MAX phase decreases while secondary phases become more prevalent; the maximum Ti 3 SiC 2 content in this system is 56 vol. %. When TiSi 2 fully replaces elemental silicon in the 2.5Ti–0.5TiSi2–2C mixture, the Ti 3 SiC 2 fraction drops to 20 vol. %.

This publication has 35 references indexed in Scilit: