Permanent magnets by mechanical alloying (invited)

Authors:

Abstract
Mechanical alloying is applied to prepare Nd‐Fe‐B, Sm‐Fe‐TM type (TM: V, Ti, Zr), and interstitial nitride and carbide permanent magnets. Starting from elemental powders, the hard magnetic phases are formed by milling in a planetary ball mill and a following solid‐state reaction at relatively low temperatures. For Nd‐Fe‐B, the magnetically isotropic particles are microcrystalline, show a high coercivity (up to 16 kA/cm for ternary alloys and above for Dy‐substituted samples), and can be either used for making bonded magnets or compacted to dense isotropic magnets by hot uniaxial pressing. Magnetically anisotropic samples with a remanence up to 1.31 T and an energy product up to 326 kJ/m3 are formed by die upsetting. The mechanical alloying process has also been applied to prepare magnetic material of three new Sm‐Fe‐TM phases: Sm‐Fe‐V with the ThMn12 structure, Sm‐Fe‐Zr with the PuNi3 structure, and Sm‐Fe‐Ti with the A2 structure. They all show high or ultrahigh coercivities (up to 51.6 kA/cm for Sm‐Fe‐Ti), but their saturation magnetization is comparably low. More promising are the interstitial nitrides or carbides of the 2:17 or the 1:12 phases. Magnetically isotropic microcrystalline Sm2Fe17Nx samples with coercivities up to 24 kA/cm were prepared by mechanical alloying and a two‐step heat treatment. Their remanence and energy product are equivalent to similarly prepared Nd‐Fe‐B samples, but their properties at elevated temperatures are superior because of the high Curie temperature of 470 °C and the large anisotropy field of 22 T. Also for Sm2Fe17Cy and 1:12‐type Nd‐Fe‐V‐N, coercivities of 18.5 or 6 kA/cm, respectively, were achieved.

This publication has 21 references indexed in Scilit: