Abstract
Compared with an undoped Sb3Te film, a Zn26.28(Sb3Te)73.72 film exhibits high crystallization temperature (∼202 °C) and activation energy of crystallization (∼3.28 eV), resulting in stability at high temperatures with an extrapolated life-time of 10 years at 130 °C. The crystalline resistance increases and the amorphous/crystalline resistance ratio is about 104, which is helpful to achieve a high On/OFF ratio. The optical band gap of a Zn26.28(Sb3Te)73.72 film decreases as it transforms from the amorphous phase to the crystalline phase. The average kinetic exponent (n) of the film is 2.44, indicating that its crystallization mechanism is of the nucleation-dominated type.

This publication has 16 references indexed in Scilit: