Abstract
A silicate–apatite layer was formed on commercially available anodically oxidized titanium rods using Na2SiO3‐containing supersaturated calcium phosphate solutions. With the increase in the concentration of Na2SiO3 in the supersaturated calcium phosphate solutions, the amounts of silicon that precipitated on the titanium rods increased from 0 to 0.07 ± 0.02 μg/cm2; meanwhile, the amounts of calcium and phosphorus that precipitated on the titanium rods decreased from 11.6 ± 1.6 and 5.7 ± 2.0 μg/cm2 to 2.6 ± 0.5 and 3.0 ± 1.0 μg/cm2, respectively. The present silicate–apatite composite layers, which demonstrated increased fibroblastic proliferation and osteoblastic proliferation and differentiation in vitro, are promising as coating layers on external fixation pins for decreasing the pin tract infection rate in vivo. © 2009 Wiley Periodicals, Inc. J Biomed Mater Res, 2010