The Effect of Relative Density on the Mechanical Properties of Hot‐Pressed Cubic Li 7 La 3 Zr 2 O 12
- 18 January 2016
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 99 (4) , 1367-1374
Abstract
The effect of relative density on the hardness and fracture toughness of Al‐substituted cubic garnet Li 6.19 Al 0.27 La 3 Zr 2 O 12 ( LLZO ) was investigated. Polycrystalline LLZO was made using solid‐state synthesis and hot‐pressing. The relative density was controlled by varying the densification time at fixed temperature (1050°C) and pressure (62 MP a). After hot‐pressing, the average grain size varied from approximately 2.7–3.7 μm for the 85% and 98% relative density samples, respectively. Examination of fracture surfaces revealed a transition from inter‐ to intragranular fracture as the relative density increased. The Vickers hardness increased with relative density up to 96%, above which the hardness was constant. At 98% relative density, the Vickers hardness was equal to the hardness measured by nanoindentation 9.1 GP a, which is estimated as the single‐crystal hardness value. An inverse correlation between relative density and fracture toughness was observed. The fracture toughness increased linearly from 0.97 to 2.37 MP a√m for the 98% and 85% relative density samples, respectively. It is suggested that crack deflection along grain boundaries can explain the increase in fracture toughness with decreasing relative density. It was also observed that the total ionic conductivity increased from 0.0094 to 0.34 mS /cm for the 85%–98% relative density samples, respectively. The results of this study suggest that the microstructure of LLZO must be optimized to maximize mechanical integrity and ionic conductivity.Keywords
Funding Information
- Advanced Research Projects Agency - Energy (DE‐AR0000399)
- U.S. Army Research Laboratory
- U.S. Department of Energy (DE‐EE‐00006821)
- National Research Foundation of Korea (NRF‐2014R1A2A1A11052513, NRF‐2012K1A3A1A12054894)
This publication has 46 references indexed in Scilit:
- Effect of substitution (Ta, Al, Ga) on the conductivity of Li7La3Zr2O12Journal of Power Sources, 2012
- High lithium ionic conductivity in the garnet-type oxide Li7−X La3(Zr2−X, NbX)O12 (X=0–2)Journal of Power Sources, 2011
- Inorganic solid Li ion conductors: An overviewSolid State Ionics, 2009
- An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experimentsJournal of Materials Research, 1992
- Effect of Grain Size and Poling on the Fracture Mode of Lead Zirconate Titanate CeramicsJournal of the American Ceramic Society, 1990
- Effect of Sintering Atmosphere on Densification of MgO‐Doped Al 2 O 3Journal of the American Ceramic Society, 1988
- Review Lecture - Fast ionic conduction in solidProceedings of the Royal Society of London. A. Mathematical and Physical Sciences, 1984
- Intergranular Crack‐Deflection Toughening in Silicon CarbideJournal of the American Ceramic Society, 1983
- A Critical Evaluation of Indentation Techniques for Measuring Fracture Toughness: I, Direct Crack MeasurementsJournal of the American Ceramic Society, 1981
- Grain‐Size Dependence of Fracture Energy in Ceramics: I, ExperimentJournal of the American Ceramic Society, 1981