Sulfuric acid dew point is an important parameter in coal-fired power plants as it affects many equipments, materials, and pipes, including filter bags. This article puts forward a new method to test the effect of different sulfuric acid dew points on the performance of polyphenylene sulfide (PPS) needle felt. Oxidation reaction mechanisms were predicted using Fourier transform infrared analysis. The results show that the degradation starts with S atoms in the PPS molecular chain; first, the thioether bond is broken, followed by sulfonation of benzene, and finally concluding with the carbonization of PPS. Furthermore, PPS thermal properties also show a decrease in the melting temperatures and thermal decomposition temperatures as well as an increase in the residual mass of the initial weight with increasing sulfuric acid dew point. Changes in the thermal properties of PPS further confirmed that different reaction mechanisms exist under different acid dew points.Keywords
This publication has 6 references indexed in Scilit:
- Polyphenylene sulfide (PPS) composites reinforced with recycled carbon fiberComposites Science and Technology, 2013
- Synthesis and characterization of nitrated and aminated poly(phenylene sulfide) derivatives for advanced applicationsMaterials Chemistry and Physics, 2012
- Mechanical degradation of filter polymer materials: Polyphenylene sulfidePolymer Degradation and Stability, 2006
- Degradation of semi-crystalline PPS bag-filter materials by NO and O2 at high temperaturePolymer Degradation and Stability, 2006
- Thermal decomposition characteristics of poly(phenylene sulfide) by stepwise Py-GC/MS and TG/MS techniquesPolymer Degradation and Stability, 2000
- Polyphenylene Sulfide (PPS) in Harsh Environments1983