Marginal fit of heat pressed lithium disilicate crowns fabricated by three-dimensional printed and subtractive CAD/CAM wax patterns

Authors:

Abstract
Purpose This study was performed to evaluate the effect of different methods of fabrication of wax pattern on the marginal adaptation of heat pressed lithium disilicate crown restorations. Materials and methods Three techniques were used for wax pattern fabrication, the first group was three-dimensional (3D) printed, the second group was subtractive and the third was conventional technique (control group). Ten samples were fabricated using each technique. USB digital microscope with a built-in camera was used to capture the photos of the margins and a digital image analysis system was used to measure and qualitatively evaluate the gap width by selecting eight eqidistant points along the margin and measuring the gap at each point. Results F-test (analysis of variance) was used to compare between more than two groups, and post-hoc test (LSD) for pairwise comparisons. The overall mean marginal gap for the three groups 3D, subtractive and conventional was 40.33 ± 0.77, 42.18 ± 1.44 and 43.13 ± 1.15, respectively. Post-hoc test (LSD) revealed a significant difference between 3D and subtractive group (P = 0.001) and it revealed a highly significant difference between 3D and conventional group (P < 0.001). However, post-hoc test revealed no significant difference between subtractive and conventional group (P = 0.076). Conclusion The 3D printed group has higher marginal fit than the other two groups. Research hypotheses: There is a difference in the marginal fit of heat pressed lithium disilicate crown restorations fabricated using 3D printed, subtractive and conventional wax pattern.

This publication has 2 references indexed in Scilit: