Influence of bioactive glass S53P4 granules and putty on osteomyelitis associated bacteria in vitro
Authors:
- Patricia StoorPSPatricia Stoor
- Janek FrantzenJFJanek Frantzen
Open Access
- 9 November 2017
- journal article
- research article
- Published by Portico in Biomedical glasses
- Vol. 3 (1) , 79-85
Abstract
Bacterial infection of bone tissue and bone marrow, referred to as osteomyelitis, is a challenging clinical problem. In this study we analysed the influence of the granule size of the bone substitute bioactive glass (BAG) S53P4 and the novel putty material containing BAG S53P4 on four clinically important bacteria associated with osteomyelitis; Staphylococcus aureus, methicillin resistant Staphylococuus aureus, Staphylococcus epidermidis and Pseudomonas aeruginosa. Reference materials were the frequently used biomaterial in surgical bone grafting procedures; tricalcium phosphate and an inert glass. Powder of BAG S53P4 was used as a positive control. The materials were incubated with bacterial suspension and the viability of the microbeswas determined as colony forming units after cultivation on agar plates. All pathogens lost their viability in contact with the BAG S53P4 granules and the powder of the BAG S53P4. The reference materials tricalcium phosphate and the inert glass had no effect on the viability of the bacteria. The BAG S53P4 putty containing 0.5-0.8 mm granules did not show any antibacterial effect on any of the tested bacteria. New putty compositions need to be investigated to obtain antibacterial properties for this novel bone regeneration biomaterial.Keywords
This publication has 14 references indexed in Scilit:
- A comparative study of the use of bioactive glass S53P4 and antibiotic-loaded calcium-based bone substitutes in the treatment of chronic osteomyelitisThe Bone & Joint Journal, 2014
- The use of Antimicrobial-Impregnated PMMA to Manage Periprosthetic Infections: Controversial Issues and the Latest DevelopmentsThe International Journal of Artificial Organs, 2012
- Posterolateral Spondylodesis Using Bioactive Glass S53P4 and Autogenous Bone in Instrumented Unstable Lumbar Spine Burst FracturesScandinavian Journal of Surgery, 2012
- Instrumented Spondylodesis in Degenerative Spondylolisthesis With Bioactive Glass and Autologous BoneJournal of Spinal Disorders & Techniques, 2011
- Detection of Streptococcus pneumoniae carriage by the Binax NOW test with nasal and nasopharyngeal swabs in young childrenEuropean Journal of Clinical Microbiology & Infectious Diseases, 2011
- Antibacterial effect of bioactive glasses on clinically important anaerobic bacteria in vitroJournal of Materials Science: Materials in Medicine, 2007
- Bactericidal effects of bioactive glasses on clinically important aerobic bacteriaJournal of Materials Science: Materials in Medicine, 2007
- Molecular Basis for Action of Bioactive Glasses as Bone Graft SubstituteScandinavian Journal of Surgery, 2006
- Pathogenesis of infections due to coagulasenegative staphylococciThe Lancet Infectious Diseases, 2002
- Antibacterial effects of a bioactive glass paste on oral microorganismsActa Odontologica Scandinavica, 1998